C-24
WELDED PANEL REPLACEMENT -

REAR DOOR OUTER PANEL

REPAIR WELDS
A
: Adhesive
Adhesive
Type
Chloroprene-base drying sealant
NOTE
After hemming the rear door outer panel, MIG spot weld the flange overlap section at a pitch of 50
mm.
Symbol
B
C
Rear Door Outer Panel
Operation description
Spot welding
MIG plug welding (
: indicates two panels to be
J
welded
: indicates three panels to be welded)
Y
MIG spot welding
MIG arc welding (continuous)
Braze welding
Anti-corrosion agent application locations
(Use access holes to apply liberally to butt-welded
joints.)
50 mm
A
B
C